SAE AMS4902K
Titanium Sheet, Strip, and Plate Commercially-Pure Annealed 40.0 ksi (276 MPa) Yield Strength
standard by SAE International, 08/26/2013
- Comments Off on SAE AMS4902K
- SAE
Titanium Sheet, Strip, and Plate Commercially-Pure Annealed 40.0 ksi (276 MPa) Yield Strength
standard by SAE International, 08/26/2013
Copper, Sheet, Strip, and Plate Soft Annealed
standard by SAE International, 09/21/2017
Titanium Alloy, Sheet, Strip, and Plate 6Al – 4V Annealed
standard by SAE International, 02/22/2018
Bearings, Babbitt 91Sn – 4.5Sb – 4.5Cu
standard by SAE International, 02/15/2012
Aluminum Bronze Bars, Rods, and Forgings 87Cu ¿¿¿ 9Al – 3Fe Stress Relieved
standard by SAE International, 06/18/2015
Aluminum Alloy, Plate (7140-T7651) 6.6Zn – 1.8Cu – 2.0Mg – 0.10Zr Solution Heat Treated, Stress Relieved, and Overaged
standard by SAE International, 02/12/2018
Magnesium Alloy, Sand Castings 8.7Al – 0.70Zn – 0.26Mn (AZ91E-T6) Solution and Precipitation Heat Treated
standard by SAE International, 11/14/2018
Silicon Bronze Bars, Rods, Forgings, and Tubing 92Cu – 3.2Si – 2.8Zn – 1.5Fe Stress Relieved
standard by SAE International, 02/15/2012
Copper-Nickel Alloy Wire and Ribbon, 77.5Cu – 22.5Ni
standard by SAE International, 04/13/2007
Copper-Beryllium Alloy Sheet, Strip, and Plate, 98Cu 1.9Be, Solution Heat Treated (TB00)
standard by SAE International, 12/02/2010