SAE AMS4973H
Titanium Alloy Forgings 8Al – 1Mo – 1V Solution Heat Treated and Stabilized
standard by SAE International, 08/01/2016
- Comments Off on SAE AMS4973H
- SAE
Titanium Alloy Forgings 8Al – 1Mo – 1V Solution Heat Treated and Stabilized
standard by SAE International, 08/01/2016
Aluminum Alloy, Extrusions 4.4Cu – 1.5Mg – 0.60Mn (2024-T8511) Solution Heat Treated, Cold Worked, Stress-Relieved by Stretching, Precipitation Heat Treated, and Straightened
standard by SAE International, 01/03/2019
Aluminum Alloy, Plate 3.5Cu – 1.0Li – 0.40Mg – 0.35Mn – 0.45Ag – 0.12Zr (2050-T84) Solution Heat Treated, Stress Relieved, and Artificially Aged
standard by SAE International, 05/10/2019
Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 52.5Ni – 19Cr – 3.0Mo – 5.1Cb(Nb) – 0.90Ti – 0.60Al – 18Fe Vacuum Melted Homogenization and Solution Heat Treated
standard by SAE International, 08/16/2018
Steel, Investment Castings 0.50Cr – 0.55Ni – 0.20Mo (0.25 – 0.35C) (SAE 8630 Mod) Normalized and Tempered
standard by SAE International, 04/30/2013
Magnesium Alloy Castings, Sand, 6.0Al – 3.0Zn (AZ63 – T4), Solution Heat Treated
standard by SAE International, 10/30/2006
Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 52.5Ni – 19Cr – 3.0Mo – 5.1Cb(Nb) – 0.90Ti – 0.60Al – 18Fe Vacuum Melted Homogenization and Solution Heat Treated
standard by SAE International, 10/11/2012
Solder, Tin-Lead 45Sn – 55Pb (Stabilized: Apr 2017)
standard by SAE International, 04/07/2017
Alloy Bars, Corrosion and Heat Resistant, Nickel Base – 15.5Cr – 0.95 (Cb + Ta) – 2.5Ti – 0.70Al – 7.0Fe, Consumable Electrode or Vacuum Induction Melted
standard by SAE International, 07/01/1985
Steel, Corrosion Resistant, Wire 17Cr – 7.1Ni – 1.1Al Cold Drawn, Precipitation-Hardenable
standard by SAE International, 10/21/2013