SAE AMS4963D
Titanium Alloy, Bars, Wire, Forgings, and Rings 6.0Al – 4.0V Annealed, Heat Treatable, Modified Strength
standard by SAE International, 08/01/2016
- Comments Off on SAE AMS4963D
- SAE
Titanium Alloy, Bars, Wire, Forgings, and Rings 6.0Al – 4.0V Annealed, Heat Treatable, Modified Strength
standard by SAE International, 08/01/2016
Steel, Corrosion Resistant, Safety Wire, 18Cr – 11.5Ni (SAE 30305), Solution Heat Treated, Cold Finished
standard by SAE International, 08/24/2007
Alloy Powder, Corrosion and Heat Resistant, 59.5ni 12cr 10co 3.0mo 6.0w 3.0ti 1.5ta 4.5al 0.015b 0.10zr (0.30-0.35c), as Fabricated
standard by SAE International, 01/01/1993
Steel Castings, Sand and Centrifugal, Corrosion and Heat Resistant 18.5Cr – 10.5Ni – 0.90 (Cb+Ta) Solution Heat Treated
standard by SAE International, 10/11/2012
Steel, Corrosion and Heat-Resistant, Welding Wire 20.5Cr 9.0Ni 0.50Mo 1.5W 1.2Cb 0.20Ti Vacuum Induction Melted ( Reaffirmed: Apr 2007 )
standard by SAE International, 08/01/2002
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Rings 61Ni – 20.5Cr – 8.5Mo – 3.4Cb(Nb) – 1.3Ti – 5.0Fe Consumable Electrode or Vacuum Induction Melted Solution Heat Treated
standard by SAE International, 12/02/2015
Titanium Alloy, Forgings, 10V – 2Fe – 3AI, Consumable Electrode Melted, Single-Step Solution Heat Treated and Overaged, 140 ksi (965 MPa) Tensile Strength
standard by SAE International, 05/26/2011
Aluminum Alloy, Plate (7085-T7451) 7.5Zn – 1.6Cu – 1.5Mg – 0.12Zr Solution Heat Treated, Stress-Relieved, and Overaged
standard by SAE International, 12/27/2018
Steel, Bars, Forgings, and Tubing 0.80Cr (0.90 ¿¿¿ 1.03C) For Bearing Applications
standard by SAE International, 09/10/2015
Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 72Ni – 3.2Mn – 20Cr – 2.5Cb – 0.48Ti Vacuum Induction Melted, Environment Controlled Packaging
standard by SAE International, 12/04/2015