SAE AMS5080J

Steel, Bars, Forgings, and Tubing, 0.31 – 0.38C (SAE 1035)
standard by SAE International, 02/20/2006

SAE AMS4988B

Titanium Alloy Sheet, Strip, and Plate, 6Al – 6V – 2Sn, Solution Heat Treated
standard by SAE International, 02/07/2013

SAE AMS6374D

Steel Tubing, Seam-Free, Round 0.95Cr – 0.20Mo (0.28 – 0.33C) (SAE 4130) 95.0 ksi (655 MPa) Tensile Strength
standard by SAE International, 01/12/2016

SAE AMS6350N

Steel Sheet, Strip, and Plate 0.95Cr – 0.20Mo (0.28 – 0.33C) (SAE 4130)
standard by SAE International, 12/19/2015

SAE AMS5671G

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni – 15.5Cr – 0.95Cb – 2.5Ti – 0.70Al – 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 ¿¿F (982 ¿¿C) Solution Heat Treated, Precipitation Hardenable
standard by SAE International, 11/27/2013

SAE AMS5046C

Carbon Steel, Sheet, Strip, and Plate (SAE 1020 and 1025) Annealed
standard by SAE International, 05/01/2007

SAE AMS5853D

Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr – 25.5Ni – 1.2Mo – 2.1Ti – 0.006B – 0.30V Consumable Electrode Melted 1800 ¿¿F (982 ¿¿C) Solution Treated and Work-Strengthened Capable of 160 ksi (1103 MPa) Tensile Strength
standard by SAE International, 02/04/2019

SAE AMS5442A

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni – 18Cr – 2.8Mo – 5.5Cb(Nb) – 0.70Ti – 1.50Al – 10Fe – 9Co – 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated
standard by SAE International, 09/13/2011

SAE AMS4907K

Titanium Alloy, Sheet, Strip, and Plate 6.0Al – 4.0V, Extra Low Interstitial Annealed
standard by SAE International, 09/26/2013

SAE AMS5862K

Steel, Corrosion-Resistant, Sheet, Strip, and Plate 15Cr – 4.5Ni – 0.30Cb (Nb) – 3.5Cu Consumable Electrode Remelted, Solution Heat Treated Precipitation-Hardenable
standard by SAE International, 07/08/2013