SAE AMS4785H
Gold-Palladium-Nickel Alloy Brazing Filler Metal, High Temperature, 30Au 34Pd 36Ni, 2075 to 2130°F (1135 to 1166°C) Solidus-Liquidus Range
standard by SAE International, 07/16/2009
- Comments Off on SAE AMS4785H
- SAE
Gold-Palladium-Nickel Alloy Brazing Filler Metal, High Temperature, 30Au 34Pd 36Ni, 2075 to 2130°F (1135 to 1166°C) Solidus-Liquidus Range
standard by SAE International, 07/16/2009
Titanium Alloy, Bars, Wire, and Rings 6.0Al – 2.0Sn – 4.0Zr – 2.0Mo – 0.08Si Solution and Precipitation Heat Treated
standard by SAE International, 03/07/2014
Steel, Corrosion and Heat-Resistant, Seamless Tubing 25Cr – 20Ni (SAE 30310S) Solution Heat Treated
standard by SAE International, 07/31/2019
Silver Alloy, Brazing Filler Metal 45Ag – 24Cd – 16Zn – 15Cu 1125 to 1145 ¿¿F (607 to 618 ¿¿C) Solidus-Liquidus Range (Stabilized: Dec 2015)
standard by SAE International, 12/08/2015
Aluminum Alloy, Extruded Profiles (2824-T3511) 4.0Cu – 1.35Mg – 0.7Mn Solution Heat Treated and Stress Relieved by Stretching
standard by SAE International, 01/05/2015
Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant Nickel Base – 15.5Cr – 16Mo – 3.8W – 5.5Fe Solution Heat Treated
standard by SAE International, 04/12/2012
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni – 18Cr – 2.8Mo – 5.5Cb(Nb) – 0.70Ti – 1.50Al – 10Fe – 9Co – 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 ¿¿F (968 ¿¿C) Solution Heat Treated, Precipitation-Hardenable
standard by SAE International, 11/22/2016
Steel Castings, Sand, 0.65Cr – 0.75Ni – 0.20Mo (0.25 – 0.33C) (SAE 8630 Modified) Normalized and Tempered
standard by SAE International, 10/01/2001
Tin Bronze Castings, Sand and Centrifugal, 87.5Cu – 10Sn – 2Zn, As Cast
standard by SAE International, 10/23/2009
Magnesium Alloy Castings, Sand, 3.3Th – 0.75Zr (HK31A-T6), Solution and Precipitation Heat Treated
standard by SAE International, 06/21/2006