SAE AMS5365E
Steel Castings, Sand, Corrosion and Heat Resistant 24.5Cr – 20.5Ni Solution Heat Treated
standard by SAE International, 07/30/2019
- Comments Off on SAE AMS5365E
- SAE
Steel Castings, Sand, Corrosion and Heat Resistant 24.5Cr – 20.5Ni Solution Heat Treated
standard by SAE International, 07/30/2019
Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb (Nb) 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated For Work Strengthening
standard by SAE International, 08/01/2006
Aluminum Alloy Plate (2624-T39) 4.1Cu – 1.4Mg – 0.6Mn Solution Heat Treated, Cold Worked and Naturally Aged
standard by SAE International, 09/13/2011
Steel, Bars, Forgings, and Tubing 1.6Si – 0.82Cr – 1.8Ni – 0.40Mo – 0.08V (0.38 – 0.43C) Consumable Electrode Vacuum Remelted
standard by SAE International, 07/08/2015
Alloy Castings, Corrosion and Heat-Resistant 66Ni – 29Cu – 4.0Si Solution Treated
standard by SAE International, 08/25/2017
Magnesium Alloy, Sand Castings 4.2Zn – 1.2 Rare Earths – 0.7Zr (ZE41A-T5) Precipitation Heat Treated
standard by SAE International, 12/27/2018
Steel, Bars and Forgings 0.90Si – 1.0Cr – 2.0Ni – 3.2Mo – 2.0Cu – 0.10V (0.07 – 0.13C) Vacuum Arc or Electroslag Remelted
standard by SAE International, 05/16/2018
Alloy Castings, Investment, Corrosion and Heat Resistant, 63Ni – 8.0Cr – 10Co – 6.0Mo – 1.0Ti – 4.2Ta – 6.0Al – 0.015B – 0.03Zr – 1.2Hf, Vacuum Melted, Vacuum Cast, As Cast
standard by SAE International, 04/05/2007
Nickel-Copper Alloy, Corrosion-Resistant, Bars and Forgings 67Ni – 30Cu
standard by SAE International, 01/04/2011
Aluminum Alloy, Plate 4.0Cu – 1.0Li – 0.40Mg – 0.35Ag – 0.13Zr (2195-T34) Solution Heat Treated and Stress Relieved
standard by SAE International, 06/06/2011