SAE AMS5843G

Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars 19Cr – 36Co – 25Ni – 7.0Mo – 0.50Cb (Nb) – 2.9Ti – 0.20Al – 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged
standard by SAE International, 06/06/2016

SAE AMS6905C

Titanium Alloy Bars, Forgings and Forging Stock 6.0Al – 2.0Sn – 4.0Zr – 2.0Mo Duplex Annealed
standard by SAE International, 07/25/2018

SAE AMS6494B

Steel Bars, Forgings, and Tubing 1.0Cr ¿¿¿ 2.50Ni ¿¿¿ 2.0Mo ¿¿¿ 1.10Si (0.10 ¿¿¿ 0.20C) Aircraft-Quality
standard by SAE International, 06/30/2016

SAE AMS5574F

Steel, Corrosion and Heat Resistant, Seamless Tubing 23Cr – 13.5Ni (309S) Solution Heat Treated
standard by SAE International, 07/31/2019

SAE AMS5720A

Steel, Corrosion and Heat Resistant 20cr 9ni 1.4mo 1.4w
standard by SAE International, 01/01/1982

SAE AMS6515B

Steel, Maraging, Bars, Forgings, Tubing, and Rings 18.5Ni – 12.0Co – 4.9Mo – 1.40Ti – 0.10Al Double Vacuum Melted, Annealed
standard by SAE International, 07/18/2018

SAE AMS5592E

Iron-Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 44Fe 18.5Cr 35Ni 1.15Si, Solution Heat Treated ( Reaffirmed: Oct 2006 )
standard by SAE International, 01/01/2002

SAE AMS5583D

Nickel Alloy, Corrosion and Heat Resistant, Seamless Tubing 72Ni 15.5Cr 0.95Cb 2.5Ti 0.70Al 7.0Fe, Vacuum Melted Solution Heat Treated, Precipitation Hardenable to 170 ksi (1172 MPa) Tensile Strength ( Reaffirmed: Oct 2006 )
standard by SAE International, 03/01/2002

SAE AMS6413M

Steel, Mechanical Tubing 0.80Cr – 1.8Ni – 0.25Mo (0.35 – 0.40C) (4337)
standard by SAE International, 01/19/2016

SAE AMSS5000A

Steel, Chrome-Nickel-Molybdenum (E4340) Bars and Reforging Stock
standard by SAE International, 03/01/2007