SAE AMS5047G

Steel, Sheet and Strip 0.08 – 0.13C, Aluminum Killed (SAE 1010) Deep Forming Grade (Stabilized: Feb 2017)
standard by SAE International, 02/15/2017

SAE ARP1940A

Solid-State Frequency Converter, 400 Hertz, 3-Phase Output
standard by SAE International, 03/07/2012

SAE AMS4916K

Titanium Alloy Sheet, Strip, and Plate 8Al – 1Mo – 1V Duplex Annealed
standard by SAE International, 02/27/2014

SAE AMS4418G

Magnesium Alloy, Sand Castings, 2.5Ag 2.1Di 0.70Zr (QE22A-T6), Solution and Precipitation Heat Treated
standard by SAE International, 11/24/2004

SAE AMS5046E

Carbon Steel, Sheet, Strip, and Plate (SAE 1020 and 1025)
standard by SAE International, 05/09/2017

SAE AMS5592E

Iron-Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 44Fe 18.5Cr 35Ni 1.15Si, Solution Heat Treated ( Reaffirmed: Oct 2006 )
standard by SAE International, 01/01/2002

SAE AMS5583D

Nickel Alloy, Corrosion and Heat Resistant, Seamless Tubing 72Ni 15.5Cr 0.95Cb 2.5Ti 0.70Al 7.0Fe, Vacuum Melted Solution Heat Treated, Precipitation Hardenable to 170 ksi (1172 MPa) Tensile Strength ( Reaffirmed: Oct 2006 )
standard by SAE International, 03/01/2002

SAE ARP1834B

Fault/Failure Analysis For Digital Systems and Equipment (Stabilized: Feb 2018)
standard by SAE International, 02/14/2018

SAE AMS6527E

Steel, Bars and Forgings 2.0Cr – 10Ni – 14Co – 1.0Mo (0.15 – 0.19C) Vacuum Melted, Normalized and Overaged
standard by SAE International, 08/09/2013

SAE AMS6430H

Steel, Bars, Forgings, Tubing, and Rings 0.75Mn – 0.78Cr – 1.8Ni – 0.35Mo – 0.20V (0.32 – 0.38C) (4335 Modified)
standard by SAE International, 09/13/2012