SAE AMS6906B
Titanium Alloy Bars, Forgings, and Forging Stock 6.0Al – 2.0Sn – 4.0Zr – 6.0Mo Solution Heat Treated and Aged
standard by SAE International, 06/01/2015
- Comments Off on SAE AMS6906B
- SAE
Titanium Alloy Bars, Forgings, and Forging Stock 6.0Al – 2.0Sn – 4.0Zr – 6.0Mo Solution Heat Treated and Aged
standard by SAE International, 06/01/2015
Nickel Alloy, Corrosion and Heat Resistant, Forgings, 55Ni – 15Cr – 17Co – 5.0Mo – 3.5Ti – 4.0Al – 0.025B, Solution, Stabilization, and Precipitation Heat Treated, Powder-Metallurgy Product
standard by SAE International, 05/15/2006
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 19Cr – 10Ni Solution Heat Treated
standard by SAE International, 01/19/2017
Steel, Corrosion-Resistant, Investment Castings 15Cr – 4.6Ni – 0.22Cb (Nb) – 2.8Cu Solution and Precipitation Heat Treated (H925) 180 ksi (1241 MPa) Tensile Strength (15-5)
standard by SAE International, 04/09/2014
Titanium Alloy Bars, Wire, and Forgings, 6.0Al – 2.0Sn – 4.0Zr – 6.0Mo, Solution and Precipitation Heat Treated
standard by SAE International, 09/14/2012
Titanium Alloy Bars, Wire, and Forgings 7Al – 4Mo Solution and Precipitation Heat Treated
standard by SAE International, 09/25/2012
Gold-Palladium-Nickel Alloy, Brazing Filler Metal, High Temperature 50Au – 25Pd – 25Ni 2015 to 2050 ¿¿F (1102 to 1121 ¿¿C) Solidus-Liquidus Range
standard by SAE International, 10/10/2018
Propeller Attachment – Nose Mounted ( Reaffirmed: Feb 1984 Jul 1991 May 1995 Nov 2001 Jul 2006 )
standard by SAE International, 04/01/1960
Tubing, Plastic, Flexible, Convoluted, Fluorinated Ethylene Propylene, Integral Braid
standard by SAE International, 03/16/2011
Titanium Alloy, Bars, Wire, Forgings, Rings, and Drawn Shapes, 4Al – 2.5V – 1.5Fe, Annealed, Heat Treatable