SAE AMS6325J
Steel, Bars and Forgings 0.50Cr – 0.55Ni – 0.25Mo (0.38 – 0.43C) (SAE 8740) Heat Treated, 105 ksi (724 MPa) Tensile Strength
standard by SAE International, 04/19/2010
- Comments Off on SAE AMS6325J
- SAE
Steel, Bars and Forgings 0.50Cr – 0.55Ni – 0.25Mo (0.38 – 0.43C) (SAE 8740) Heat Treated, 105 ksi (724 MPa) Tensile Strength
standard by SAE International, 04/19/2010
Steel Bars and Forgings, Low Alloy, Heat-Resistant 0.65Si – 1.25Cr – 0.50Mo – 0.85V (0.25 – 0.30C)
standard by SAE International, 08/17/2012
Optical Measurement Procedures for Airborne Head Up Display (HUD)
standard by SAE International, 01/04/2008
Anodize Treatment of Titanium and Titanium Alloys pH 12.4 Maximum (Cancelled: Jan 1985)
standard by SAE International, 01/01/1985
Aluminum Alloy, Extruded Profiles (2043-T85) 2.8Cu – 1.65Li – 0.35Mg – 0.1Zr Solution Heat Treated, Stress Relieved by Stretching, and Aged
standard by SAE International, 07/03/2019
Steel, Corrosion and Heat Resistant, Seamless Tubing 23Cr 13.5Ni (SAE 30309S) Solution Heat Treated ( Reaffirmed: Apr 2006 )
standard by SAE International, 06/01/2001
Pallet/Container Loader Auto-Levelling Systems
standard by SAE International, 09/28/2016
Titanium Alloy Extrusions and Flash Welded Rings 6Al – 4V Annealed Beta Processed
standard by SAE International, 01/16/2014
Useful Life Determination for Chemical Oxygen Generators